How to use

Waterproofing-Coat

1. Fill cracks, clean and wet the surface

1. Fill cracks, clean and wet the surface

2. Add components A and B to water.

Ratio by weight: 1 (Liquid) : 2 (Powder) : 0.5 (Water)

2. Add components A and B to water.

Ratio by weight: 1 (Liquid) : 2 (Powder) : 0.5 (Water)

3. Mix using a blender to a homogeneous mix

3. Mix using a blender to a homogeneous mix

4. Apply two coats (One horizontal, one vertical)

After first coat, keep surface dry and traffic free for 3-6 Hrs. Apply second coat.

4. Apply two coats (One horizontal, one vertical)

After first coat, keep surface dry and traffic free for 3-6 Hrs. Apply second coat.

5. Add protective screed/plaster

After three days of air curing of second coat

5. Add protective screed/plaster

After three days of air curing of second coat

1. Fill cracks, clean and wet the surface

2. Add components A and B to water.

Ratio by weight: 1 (Liquid) : 2 (Powder) : 0.5 (Water)

3. Mix using a blender to a homogeneous mix

4. Apply two coats (One horizontal, one vertical)

After first coat, keep surface dry and traffic free for 3-6 Hrs. Apply second coat.

5. Add protective screed/plaster

After three days of air curing of second coat

5. Add protective screed/plaster

After three days of air curing of second coat

45

mins

POT LIFE

90-100%

ELONGATION

10

sq. ft./kg

COVERAGE

2 Coats - 1 mm Total Thickness

Application Video